Refractory Spray Coating


Product introduction

The lightweight spray-applied refractory material is manufactured primarily from expanded vermiculite, making it suitable for application in areas of the new dry-process rotary kiln that are subject to attack by alkaline gases, and can replace the calcium silicate boards originally specified in the kiln design.

Product details


Project/Grade

Lightweight spray patching material

KYSL-PB1.0

Al 2 O 3%

20-30

Fe 2 O 3%

8-12

CaO%

12-18

Silicon dioxide 2%

35-45

Bulk Density B.D g/cm 3

110℃ for 24 hours

1.0–1.3

Compressive strength C.C.S MPa, ≥

110℃ for 24 hours

4.0

500℃ for 3 hours

4.0

800℃ for 3 hours

3.0

 

1000℃ for 3 hours

2.5

Line change rate P.L.C%

500℃ for 3 hours

0 to -0.3

 

800℃ for 3 hours

0 to -0.4

 

1000℃ for 3 hours

0 to -0.9

Thermal conductivity, ≤

500°C

0.29

 

800°C

0.31

 

1000℃

0.38

Maximum operating temperature (°C)

1140

Part used

Thermal insulation layer (preheater, decomposition furnace, tertiary air duct, kiln door hood, cooler, etc.)