Low-Creep Series for Hot Blast Stoves


Product introduction

Product details


 

Project

DRL-155

DRL-150

DRL-145

DRL-140

DRL-135

DRL-130

DRL-127

Al 2 O 3,≥

75

75

65

65

65

60

50

Fe 2 O 3 %,≤

1.3

1.3

1.3

1.5

1.5

1.5

1.8

Apparent porosity A.P%, ≤

20

21

21

22

22

22

23

Bulk Density B.D g/cm 3 , ≥

2.65

2.65

2.5

2.4

2.35

2.3

2.3

Compressive strength C.C.S MPa, ≥

60

60

60

55

55

55

50

High-temperature creep rate (0.2 MPa × 50 h) %

1500℃

0.8

1500℃

0.8

1450°C

0.8

1400°C

0.8

1350℃

0.8

1300℃

0.8

1280℃

0.8

Reburning line variation rate P.L.C%

1550℃ for 2 hours

+0.1

-0.2

+0.1

-0.2

+0.1

-0.2

+0.1

-0.2

-

-

-

1450℃ for 2 hours

-

-

-

-

+0.1

-0.4

+0.1

-0.4

+0.1

-0.4

Keywords:

Online message

Leave a message now and we will arrange a specialist to contact you as soon as possible